Black & Tan Clay

Alternate Names: Blank and Tan Clay, Ball & Tan Ball Clay

Description: Originally from HC Spinks in 1970s

Oxide Analysis Formula Tolerance
CaO 0.42% 0.04
K2O 1.01% 0.05
MgO 0.37% 0.04
Na2O 0.43% 0.03
TiO2 0.36% 0.02
Al2O3 21.65% 1.00
SiO2 64.75% 5.08
Fe2O3 1.60% 0.05
LOI 9.39%n/a
SO3 0.08%n/a
Oxide Weight 426.80
Formula Weight 471.44

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy