Bell Feldspar

Description: Potash Feldspar

Oxide Analysis Formula Tolerance
CaO 0.40% 0.04
K2O 10.07% 0.65
Na2O 3.09% 0.30
Al2O3 17.87% 1.07
SiO2 68.28% 6.93
Fe2O3 0.08% -
LOI 0.21%n/a
Oxide Weight 609.02
Formula Weight 610.30