Bedminster Ball Clay

Description: Legacy ball clay from United Clay Mines

Oxide Analysis Formula Tolerance
SiO2 52.10% 2.72
Al2O3 32.50% 1.00
Fe2O3 1.50% 0.03
TiO2 1.30% 0.05
CaO 0.20% 0.01
MgO 0.50% 0.04
K2O 0.50% 0.02
Na2O 2.20% 0.11
LOI 9.10%n/a
Oxide Weight 284.97
Formula Weight 313.50

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

Data

% < 0.5 microns 66%
Drying Shrinkage 5.0%
Firing Shrinkage 10% at cone 9

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy