Alternate Names: Celsian
Formula: BaAl2Si2O8
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 40.84% | 1.00 | |
| Al2O3 | 27.16% | 1.00 | |
| SiO2 | 32.01% | 2.00 | |
| Oxide Weight | 375.40 | ||
| Formula Weight | 375.40 | ||
| URLs |
http://www.webmineral.com/data/Celsian.shtml
Celsian at Webmineral.com |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |