| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 77.40% | 1.00 | |
| B2O3 | 22.60% | 0.64 | |
| Oxide Weight | 198.06 | ||
| Formula Weight | 198.06 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |