Arcano Kaolin

Description: Plastic kaolin

Oxide Analysis Formula Tolerance
CaO 0.19% 0.01
MgO 0.18% 0.01
K2O 0.22% 0.01
Na2O 0.04% -
TiO2 0.17% 0.01
Al2O3 33.80% 1.00
SiO2 52.10% 2.62
Fe2O3 0.35% 0.01
LOI 12.90%n/a
Oxide Weight 262.70
Formula Weight 301.60

Notes

A New Zealand material.

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.