Albite and Orthoclase Eutectic

Oxide Analysis Formula Tolerance
Na2O 6.80% 0.59
K2O 7.10% 0.41
Al2O3 19.00% 1.01
SiO2 67.10% 6.03
Oxide Weight 540.40
Formula Weight 540.40

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1160C