A B Abuja Clay

Oxide Analysis Formula Tolerance
CaO 0.91% 0.16
K2O 2.87% 0.30
MgO 1.66% 0.41
Na2O 0.76% 0.12
TiO2 0.95% 0.12
Al2O3 21.31% 2.09
SiO2 55.40% 9.21
Fe2O3 7.77% 0.48
LOI 8.36%n/a
Oxide Weight 915.04
Formula Weight 998.52

Related Information

Links

Hazards Manganese Inorganic Compounds Toxicology
Hazards Occupational Dermatoses
Discussion as related to hazards encountered in the ceramic industry and process
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Data

Dry M.O.R. (50% Silica) 620C