M-75 Enamel

Oxide Analysis Formula Tolerance
CaO 0.70% 0.05
K2O 0.60% 0.02
MgO 0.90% 0.09
Na2O 0.20% 0.01
TiO2 2.19% 0.10
Al2O3 26.77% 1.00
SiO2 57.44% 3.64
Fe2O3 1.40% 0.03
LOI 9.79%n/a
Oxide Weight 343.68
Formula Weight 380.98