LM1 Ball Clay

Description: WBB Devon Ball Clay Group 1

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 1.80% 0.06
MgO 0.30% 0.02
Na2O 0.20% 0.01
TiO2 0.90% 0.03
Al2O3 33.90% 1.00
SiO2 49.40% 2.47
Fe2O3 1.00% 0.02
LOI 12.40%n/a
C 1.80%n/a
Oxide Weight 263.58
Formula Weight 307.20

Notes

Particle Size (e.s.d.)
125 microns - 0.40
10 microns - 98
2 microns - 84
1 microns - 74
Modulus of Rupture at 110C
Mn/M2 - 3.9
lbf/in2 - 570
Defloculant Required - (3:1 Na2SiO3(C.100):Na2CO3) - 0.3
Water Absorption
1120C - 9.0
1220C - 1.00
Shrinkage Dry to Fired
1120C - 14.00
1220C - 17.50
Reflectance 464nm
1120C - 72
1220C - 57
Refractoriness
Cone - 33, 1730C

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.