Alternate Names: KT Cast Kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.09% | - | |
| K2O | 0.10% | - | |
| MgO | 0.09% | 0.01 | |
| Na2O | 0.09% | - | |
| TiO2 | 1.64% | 0.05 | |
| Al2O3 | 38.80% | 1.00 | |
| SiO2 | 45.10% | 1.97 | |
| Fe2O3 | 0.50% | 0.01 | |
| LOI | 13.60% | n/a | |
| Oxide Weight | 227.16 | ||
| Formula Weight | 262.92 | ||
A coarse-grained, white-firing kaolin used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.
Physical Properties
===================
Dry M.O.R. (50:50 kaolin:silica; MnM-2): 1.6
pDry M.O.R. (50:50 kaolin:silica; psi): 225
pH: 5.5
M.B.I. (meq/100g): 2.5
Specific Surface Area (sq-m/g): 12.0
Particle Size
+325 mesh $ retained: 5.0
< 20 microns: 95%
<10 microns: 87
<5 microns: 75
<2 microns: 60
<1 micron: 41
<0.5 microns: 21
*This data is from a Jan 2013 data sheet
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |