1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Kaopaque 20 Kaolin

Alternate Names: Kaopaque, Kaopaque Kaolin

Description: White Non Plastic Delaminated Kaolin

Oxide Analysis Formula Tolerance
CaO 0.21% 0.01
K2O 0.08% -
MgO 0.03% -
Na2O 0.03% -
TiO2 0.66% 0.02
Al2O3 39.30% 1.00
SiO2 45.20% 1.95
Fe2O3 0.32% 0.01
LOI 12.00%n/a
Oxide Weight 222.76
Formula Weight 253.14

Notes

A white firing delaminated material of low plasticity. Kaopaque 20 and 10 are non-predispersed from a water-fractionated feed for a controlled particle size and shape (very large plate-like). It is refined from Geogia deposits. Kaopaque 10S is the pre-dispersed version and is supplied as a lightly pulverized spray-dried powder and as a slurry. The large plate-like particles of Kaopaque 10 have a thickness of 0.2 to 0.4 microns and a diameter of 2 to 10 microns.

Kaopaque is useful in casting porcelains. It fires white compared to other North American kaolins (because of its low Fe2O3 and TiO2), but others available internationally are much whiter (e.g. New Zealand halloysite, Grolleg kaolin, they have higher Fe2O3 but their TiO2 levels are more than ten times lower). Kaolins of higher iron content, like Opticast, also work well for slip casting and cost much less.

Kaopaque 20 has very high fired shrinkage (from 10-12% from cone 8-10), happening inspite of the fact that it is very refractory (15% porosity at cone 8, 10% at cone 10).

Related Information

Links

URLs http://www.fitzchem.com/
More information
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy