| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.90% | 0.32 | |
| K2O | 0.60% | 0.01 | |
| MgO | 10.30% | 0.58 | |
| Na2O | 2.40% | 0.09 | |
| TiO2 | 1.60% | 0.05 | |
| Al2O3 | 14.10% | 0.31 | |
| P2O5 | 0.30% | - | |
| SiO2 | 48.60% | 1.82 | |
| Fe2O3 | 11.20% | 0.16 | |
| MnO | 0.10% | - | |
| LOI | 3.80% | n/a | |
| Oxide Weight | 218.89 | ||
| Formula Weight | 227.54 | ||
Volcanic rock essentially of plagioclase, labradorite, magnetite, and pyroxene, with olivine, biotite, and hornblende. Formed by magma emission. There are two distinct basalts: feldspathic and alkaline, both plagioclase feldspathics but the latter containing significantly more sodium and potassium.

This picture has its own page with more detail, click here to see it.
Basalt

This picture has its own page with more detail, click here to see it.
Peridot In Basalt
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk