1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

K-40 Feldspar

Description: POTASH/SODIUM/CALCIUM FELDSPAR

Oxide Analysis Formula Tolerance
CaO 0.17% 0.02
K2O 10.60% 0.66
MgO 0.05% 0.01
Na2O 3.30% 0.31
Al2O3 17.88% 1.03
SiO2 67.34% 6.59
Fe2O3 0.08% -
LOI 0.19%n/a
Oxide Weight 584.74
Formula Weight 585.86

Notes

K-40 is used as a source of alumina and potash in specialized glass batch formulations requiring high potassium levels. Carefully beneficiated using the froth floation process, K-40 Feldspar offers low iron and high alkali content per unit of alumina.

Screen Analysis (Cum %):
+30 mesh: 0.1
+40 mesh: 0.22
+200 mesh: 95.9

Bulk Density: 90 lbs/cu ft

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy