IXL RE

Description: KAOLINIZED SAND

Oxide Analysis Formula Tolerance
CaO 0.22% 0.03
K2O 2.93% 0.25
MgO 0.36% 0.07
Na2O 0.36% 0.05
TiO2 0.49% 0.05
Al2O3 12.46% 1.00
P2O5 0.05% -
SiO2 79.44% 10.82
Fe2O3 0.73% 0.04
MnO 0.02% -
LOI 3.71%n/a
Oxide Weight 794.55
Formula Weight 825.17

Notes

Pre-96 Analysis.
CaO... 0.22
K2O... 2.93
MgO... 0.36
Na2O.. 0.36
TiO2.. 0.49
Al2O3. 12.46
SiO2.. 79.44
Fe2O3. 0.73
LOI... 3.71

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.