Ione Calcine

Description: Refractory Aggregate

Oxide Analysis Formula Tolerance
CaO 0.10% -
K2O 0.15% -
MgO 0.10% 0.01
Na2O 0.15% 0.01
TiO2 2.10% 0.06
Al2O3 43.50% 1.00
SiO2 53.50% 2.09
Fe2O3 0.55% 0.01
Oxide Weight 234.83
Formula Weight 234.83

Notes

Ione calcine was a high fired kaolin base refractory aggregate with excellent chemical and physical properties.

Bulk Density, gms/cc 1.68-3.36mm particle size: 2.55-2.6
True Specific Gravity, ASTM C-1365: 2.71
Apparent Porosity, ASTM C-357, %: 2-4

PCE: Orton 33-34

Related Information

Links

Typecodes Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy