Barium Nitrate

Oxide Analysis Formula Tolerance
BaO 58.70% 1.00
LOI 41.30%n/a
Oxide Weight 153.30
Formula Weight 261.16

Related Information

Links

Hazards Barium Carbonate in Glazes
Hazards BARIUM and COMPOUNDS / Toxicology
Oxides BaO - Barium Oxide, Baria
URLs http://en.wikipedia.org/wiki/Barium_nitrate
Barium nitrate info and hazards at Wikipedia
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc14/icsc1480.htm
Barium nitrate hazards at ilo.org

Data

Dry M.O.R. (50% Silica) 1191C