Glaze Spar #56

Alternate Names: 56 Glaze Spar

Description: SODA FELDSPAR

Oxide Analysis Formula Tolerance
CaO 2.32% 0.24
K2O 4.53% 0.27
Na2O 5.33% 0.49
Al2O3 18.01% 1.01
SiO2 69.81% 6.62
Oxide Weight 570.09
Formula Weight 570.09

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.