| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.39% | 0.58 | |
| K2O | 0.05% | 0.04 | |
| Na2O | 0.28% | 0.38 | |
| Al2O3 | 0.56% | 0.46 | |
| SiO2 | 98.69% | 136.86 | |
| Fe2O3 | 0.03% | 0.02 | |
| Oxide Weight | 8,334.18 | ||
| Formula Weight | 8,334.18 | ||