March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.

Monthly Tech-Tip from Tony Hansen SignUpFeb 14-15, 2026 - Major Server Upgrade Done

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fukushima Feldspar

Oxide Analysis Formula Tolerance
CaO 0.26% 0.02
K2O 9.81% 0.56
MgO 0.23% 0.03
Na2O 4.59% 0.40
Al2O3 19.07% 1.00
Fe2O3 0.10% -
SiO2 65.15% 5.80
LOI 0.80%n/a
Oxide Weight 530.65
Formula Weight 534.93

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.