Fubasami Pyrophyllite

Oxide Analysis Formula Tolerance
K2O 0.11% 0.01
MgO 0.06% 0.01
Al2O3 18.69% 1.00
SiO2 74.76% 6.79
Fe2O3 0.22% 0.01
LOI 6.16%n/a
Oxide Weight 512.13
Formula Weight 545.75

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.