March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | Feb 14-15, 2026 - Major Server Upgrade Done | No tracking! No ads! |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.63% | 0.47 | |
| K2O | 1.09% | 0.04 | |
| Na2O | 3.41% | 0.19 | |
| SrO | 9.29% | 0.31 | |
| B2O3 | 12.49% | 0.61 | |
| Al2O3 | 9.74% | 0.33 | |
| SiO2 | 56.35% | 3.21 | |
| Oxide Weight | 342.15 | ||
| Formula Weight | 342.15 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |