Pemco Frit Pb-943

Alternate Names: Frit Pb943

Description: Low lead flux for cone 06 glazes

Oxide Analysis Formula Tolerance
CaO 6.30% 0.33
K2O 5.30% 0.16
Na2O 9.00% 0.42
PbO 6.30% 0.08
B2O3 20.30% 0.85
SiO2 52.70% 2.56
Oxide Weight 292.15
Formula Weight 292.15

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3465
Materials Hommel Frit 18
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.7 x 10-6 (40-450C)
Density (Specific Gravity) 1340
Frit Melting Range (C) 1300-1380F
I.F.P. (celsius) 547C