Pemco Frit Pb-2F35

Alternate Names: Frit Pb2F35

Description: All-fritted dinnerware glaze at Cone 1 to 4

Oxide Analysis Formula Tolerance
CaO 8.00% 0.50
K2O 1.80% 0.07
MgO 0.50% 0.04
Na2O 2.20% 0.12
PbO 17.20% 0.27
B2O3 4.30% 0.22
Al2O3 9.20% 0.31
SiO2 56.60% 3.29
Oxide Weight 348.14
Formula Weight 348.14

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3467
Materials Fusion Frit FL-17
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.90
Co-efficient of Linear Expansion 5.9 x 10-6 (50-450C)
Frit Softening Point 1650F
Frit Melting Range (C) 1600-1740F
I.F.P. (celsius) 628C