Pemco Frit Pb-1R99

Alternate Names: Frit Pb1R99

Description: High expansion lead flux for cone 06 glazes

Oxide Analysis Formula Tolerance
K2O 4.40% 0.13
Na2O 10.90% 0.47
PbO 33.30% 0.40
B2O3 12.00% 0.46
Al2O3 7.40% 0.20
SiO2 31.90% 1.43
Oxide Weight 268.76
Formula Weight 268.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 12.60
Co-efficient of Linear Expansion 12.6 x 10-6 (50-350C)
Frit Softening Point 1170F
Frit Melting Range (C) 1150-1200F
I.F.P. (celsius) 425C