Pemco Frit Pb-1151

Alternate Names: Frit Pb1151

Description: Leaded titanium frit

Oxide Analysis Formula Tolerance
CaO 3.30% 0.21
K2O 4.10% 0.15
Na2O 2.80% 0.16
PbO 30.80% 0.48
TiO2 9.00% 0.39
B2O3 6.10% 0.31
SiO2 43.90% 2.56
F 1.30% 0.24
Oxide Weight 354.81
Formula Weight 354.81

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3482
Materials Hommel Frit 27
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.5 x 10-6 (50-450C)
Frit Softening Point 1400F
Frit Melting Range (C) 1350-1450F
I.F.P. (celsius) 685C