Pemco Frit Pb-1041

Alternate Names: Frit Pb1041

Description: LEADED FRIT

Oxide Analysis Formula Tolerance
CaO 8.10% 0.42
K2O 2.50% 0.08
Na2O 1.20% 0.06
PbO 33.70% 0.44
Al2O3 5.20% 0.15
SiO2 49.30% 2.40
Oxide Weight 293.03
Formula Weight 293.03

Notes

Developed for chrome-tin pinks and maroons firing cone 02-4.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.40
Co-efficient of Linear Expansion 6.4 x 10-6 (40-450C)
Frit Softening Point 1550F
Frit Melting Range (C) 1500-1750F
I.F.P. (celsius) 640C