PotteryCrafts Frit P2960

Alternate Names: PotteryCrafts Frit 2960

Description: Low Expansion Frit

Oxide Analysis Formula Tolerance
CaO 3.70% 0.33
K2O 0.20% 0.01
Li2O 1.10% 0.19
MgO 2.20% 0.27
ZnO 3.20% 0.20
B2O3 17.60% 1.27
Al2O3 8.50% 0.42
SiO2 63.40% 5.30
Oxide Weight 502.28
Formula Weight 502.28

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 3.8
Frit Melting Range (C) 1020-1150C
By Tony Hansen