PotteryCrafts Frit P2955

Alternate Names: PotteryCrafts Frit 2955

Description: High alkali low alumina borax frit

Oxide Analysis Formula Tolerance
CaO 8.80% 0.37
K2O 8.80% 0.22
Na2O 10.90% 0.41
B2O3 13.50% 0.46
Al2O3 9.10% 0.21
SiO2 48.90% 1.91
Oxide Weight 234.69
Formula Weight 234.69

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit J
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information

Data

Co-efficient of Linear Expansion 10.9
Frit Melting Range (C) 920-1050C
By Tony Hansen