Ashinuma

Oxide Analysis Formula Tolerance
CaO 3.68% 0.49
K2O 1.85% 0.15
MgO 1.57% 0.29
Na2O 2.05% 0.25
TiO2 0.64% 0.06
Al2O3 13.61% 1.00
P2O5 0.16% 0.01
SiO2 65.51% 8.17
Fe2O3 6.47% 0.30
MnO 0.12% 0.01
LOI 4.35%n/a
Oxide Weight 716.92
Formula Weight 749.53