Pemco Frit P-802

Alternate Names: Frit 802, Frit P802

Description: Leadless flux for cone 06 glazes

Oxide Analysis Formula Tolerance
CaO 8.90% 0.44
K2O 6.90% 0.20
Na2O 8.10% 0.36
B2O3 16.50% 0.65
Al2O3 9.60% 0.26
SiO2 49.90% 2.29
Oxide Weight 275.56
Formula Weight 275.56

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3270
Materials Hommel Frit 378
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.90
Frit Melting Range (C) 1350-1450F