Pemco Frit P-1701

Alternate Names: Frit 1701, Frit P1701

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
CaO 4.70% 0.46
K2O 1.00% 0.06
Li2O 0.40% 0.07
Na2O 3.90% 0.35
SrO 1.10% 0.06
B2O3 27.00% 2.14
Al2O3 9.10% 0.49
SiO2 52.80% 4.84
Oxide Weight 551.45
Formula Weight 551.45

Notes

All-fritted glaze for high alumina bodies firing in the range of 1600-1800F.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-79
Materials Hommel Frit 487
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.40
Co-efficient of Linear Expansion 5.40 (50-450C)
Frit Softening Point 1490F
Frit Melting Range (C) 1460-1550F
I.F.P. (celsius) 612C