Johnson Matthey Frit 623

Alternate Names: Frit M623

Description: B33X7, MOK623

Oxide Analysis Formula Tolerance
BaO 9.09% 0.12
CaO 2.33% 0.09
Na2O 19.19% 0.64
ZnO 5.85% 0.15
B2O3 28.38% 0.85
Al2O3 0.29% 0.01
SiO2 34.88% 1.20
Oxide Weight 207.40
Formula Weight 207.40

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Johnson Matthey Frit 169
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy