Frit LP891

Oxide Analysis Formula Tolerance
CaO 8.83% 0.49
K2O 1.82% 0.06
MgO 0.65% 0.05
Na2O 2.59% 0.13
SrO 8.66% 0.26
B2O3 4.92% 0.22
Al2O3 10.16% 0.31
SiO2 62.38% 3.26
Oxide Weight 314.36
Formula Weight 314.36

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.