General Frit GF-27

Alternate Names: Frit 27, Frit GF27

Description: Medium lead frit cone 06-04 all-fritted hobby/artware glazes

Oxide Analysis Formula Tolerance
CaO 4.40% 0.28
Na2O 3.60% 0.21
PbO 31.50% 0.51
ZrO2 1.00% 0.03
B2O3 13.00% 0.67
Al2O3 3.40% 0.12
SiO2 43.50% 2.61
Oxide Weight 361.64
Formula Weight 361.64

Related Information

Links

Materials Pemco Frit Pb-742
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3576
Materials Fusion Frit FL-28
Materials Hommel Frit 373
Materials Ferro Frit 3493
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.90
Frit Softening Point 1400F