General Frit GF-136

Alternate Names: Frit 136, Frit GF136

Description: High Potassium

Oxide Analysis Formula Tolerance
SiO2 48.17% 2.55
B2O3 16.77% 0.77
Al2O3 12.91% 0.40
ZnO 1.02% 0.04
Na2O 13.11% 0.67
K2O 7.32% 0.25
CaO 0.71% 0.04
Oxide Weight 318.15
Formula Weight 318.15

Notes

Used in partially-fritted dinnerware and artware glazes.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.