Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit FZ-284

Alternate Names: Frit FZ284

Description: Zircon frit

Oxide Analysis Formula Tolerance
CaO 1.70% 0.20
Na2O 7.60% 0.79
ZnO 0.20% 0.02
ZrO2 11.30% 0.59
B2O3 17.10% 1.58
Al2O3 5.50% 0.35
SiO2 56.60% 6.06
Oxide Weight 643.75
Formula Weight 643.75

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-2G63
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.