Fusion Frit FZ-10

Alternate Names: Frit FZ10

Description: Zircon alkaline boro silicate frit

Oxide Analysis Formula Tolerance
CaO 1.10% 0.07
K2O 4.70% 0.18
Na2O 12.00% 0.70
ZnO 1.00% 0.04
ZrO2 12.90% 0.38
B2O3 13.20% 0.69
Al2O3 10.00% 0.36
SiO2 45.00% 2.72
Oxide Weight 362.83
Formula Weight 362.83

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit 268-D
Materials Hommel Frit 472
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy