1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-79

Alternate Names: Fusion Frit F79

Description: Low expansion flux for high alumina bodies

Oxide Analysis Formula Tolerance
CaO 4.80% 0.45
K2O 1.20% 0.07
Li2O 0.50% 0.09
Na2O 4.00% 0.34
SrO 1.00% 0.05
B2O3 26.50% 2.01
Al2O3 9.00% 0.47
SiO2 53.00% 4.66
Oxide Weight 528.41
Formula Weight 528.41

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1701
Materials Hommel Frit 487
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.72
Frit Softening Point 1500F