Fusion Frit F-496

Alternate Names: Fusion Frit F-496, Frit F496

Description: Clear Alkali Boron Frit

Oxide Analysis Formula Tolerance
Na2O 5.80% 0.85
K2O 1.60% 0.15
B2O3 16.00% 2.08
Al2O3 1.60% 0.14
SiO2 75.00% 11.29
Oxide Weight 904.70
Formula Weight 904.70

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.66
Frit Softening Point 1650F