Alternate Names: Fusion Frit F43
Description: Alkaline boron flux for high temperature glazes
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.00% | 0.43 | |
| K2O | 0.50% | 0.02 | |
| Na2O | 11.20% | 0.55 | |
| B2O3 | 22.50% | 0.98 | |
| Al2O3 | 9.50% | 0.28 | |
| SiO2 | 48.30% | 2.45 | |
| Oxide Weight | 304.36 | ||
| Formula Weight | 304.36 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.22 |
|---|---|
| Frit Softening Point | 1450F |
| By Tony Hansen Follow me on ![]() | ![]() |