Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-367

Alternate Names: Fusion Frit F367

Description: Bond Frit

Oxide Analysis Formula Tolerance
Na2O 7.80% 1.00
B2O3 38.40% 4.39
SiO2 53.80% 7.12
Oxide Weight 794.87
Formula Weight 794.87

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3185
Materials General Frit GF-143
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.18 x 10-6
Frit Softening Point 1475F
By Tony Hansen