March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.

Monthly Tech-Tip from Tony Hansen SignUpFeb 14-15, 2026 - Major Server Upgrade Done

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-280

Alternate Names: Fusion Frit F280 Fusion

Description: All fritted cone 06 glazes

Oxide Analysis Formula Tolerance
CaO 14.20% 0.68
K2O 0.60% 0.02
Na2O 7.00% 0.30
Al2O3 8.50% 0.22
B2O3 15.00% 0.58
SiO2 54.80% 2.45
Oxide Weight 268.80
Formula Weight 268.80

Notes

A popular frit used in by glaze manufacturers for the hobby ceramics market.

Related Information

Links

Materials Ferro Frit CC-250
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.9 x 10-6
Frit Softening Point 1550F
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy