Fusion Frit F-18

Alternate Names: F18 Fusion, Frit F18, Frit F 18

Description: Dinnerware Strontium Frit

Oxide Analysis Formula Tolerance
CaO 11.80% 0.59
K2O 2.40% 0.07
Na2O 2.60% 0.12
SrO 8.00% 0.22
B2O3 8.90% 0.36
Al2O3 6.80% 0.19
SiO2 59.50% 2.79
Oxide Weight 281.71
Formula Weight 281.71

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 630
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.13
Frit Softening Point 1750F
By Tony Hansen