James Kent Frit DR1328

Description: TRANSPARENT (FORMERLY #FT0541)

Oxide Analysis Formula Tolerance
BaO 1.00% 0.03
CaO 8.00% 0.64
KNaO 7.00% 0.40
ZnO 6.00% 0.33
B2O3 8.00% 0.52
Al2O3 10.00% 0.44
SiO2 58.00% 4.33
Oxide Weight 439.79
Formula Weight 439.79

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 0.308 @ 500C