Ferro Frit CM-943

Oxide Analysis Formula Tolerance
K2O 0.30% 0.01
Na2O 2.70% 0.13
PbO 43.50% 0.58
ZnO 7.60% 0.28
B2O3 5.00% 0.21
Al2O3 5.00% 0.15
SiO2 35.90% 1.78
Oxide Weight 298.51
Formula Weight 298.51

Notes

Yellow leadless cadmium, underglaze mix; complete by itself. Works well with CM-942 to produce oranges. Cone 06.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Frit Softening Point 1750F
By Tony Hansen