Description: Low zinc calcium borate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.00% | 0.71 | |
| K2O | 3.00% | 0.21 | |
| ZnO | 1.00% | 0.08 | |
| B2O3 | 15.00% | 1.43 | |
| Al2O3 | 11.00% | 0.71 | |
| SiO2 | 64.00% | 7.05 | |
| Oxide Weight | 661.88 | ||
| Formula Weight | 661.88 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |