| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.83% | 0.49 | |
| K2O | 1.82% | 0.06 | |
| MgO | 0.65% | 0.05 | |
| Na2O | 2.59% | 0.13 | |
| SrO | 8.66% | 0.26 | |
| B2O3 | 4.92% | 0.22 | |
| Al2O3 | 10.16% | 0.31 | |
| SiO2 | 62.38% | 3.26 | |
| Oxide Weight | 314.36 | ||
| Formula Weight | 314.36 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |