| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.05% | 0.01 | |
| K2O | 2.35% | 0.15 | |
| MgO | 0.28% | 0.04 | |
| TiO2 | 0.02% | - | |
| Al2O3 | 16.75% | 1.00 | |
| P2O5 | 0.01% | - | |
| SiO2 | 77.14% | 7.82 | |
| Fe2O3 | 0.42% | 0.02 | |
| MnO | 0.01% | - | |
| LOI | 2.97% | n/a | |
| Oxide Weight | 590.87 | ||
| Formula Weight | 608.96 | ||
| Dry M.O.R. (50% Silica) | 582C |
|---|