Hommel Frit 529

Description: Leadless high sodium low alumina low boron frit

Oxide Analysis Formula Tolerance
CaO 5.80% 0.26
K2O 2.10% 0.06
Na2O 16.70% 0.68
B2O3 2.60% 0.09
Al2O3 4.00% 0.10
SiO2 68.80% 2.90
Oxide Weight 253.14
Formula Weight 253.14

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts a very low temperatures.
Materials Keramikos Fritte 31.10
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.6 x 10-6 (50-450C)
Co-efficient of Linear Expansion 9.6 x 10-6
Frit Melting Range (C) 1400F